E7018 Electrode Specification & its meaning, E7018 MTC.pdf
8K views
Aug 12, 2022
Meaning of E7018 Welding Rod E7018 rod is one of the most frequently used SMAW/ stick welding low hydrogen electrodes/ rod for mild steel and Carbon Steel welding. The E7018 rod coating is made with inorganic coverings that contain minimal moisture thus providing a weld deposit with the lowest hydrogen in weldment, thus giving the