Welding of P22, P22 to Carbon Steel Welding Guidelines

What is P22- 2.25Cr-1Mo steel (F22, T22) Material?

P22 material is a 2.25Cr-1Mo (P22) steel that has important uses in the oil and gas industry. It is a low-alloy, Ferritic steel used for high temperature applications such as pressure vessels, reactors and columns.

P22 material also has high strength and toughness, making it ideal for use in applications where weight savings are important compared to carbon steel.

P22 material is a 2.25Cr-1Mo (P22) steel alloy that contains chromium and molybdenum. It is important because it offers excellent resistance to oxidation and carburization in high-temperature service.

It also has good strength and toughness, which makes it ideal for use in aircraft engines, gas turbines, and other high-temperature applications.

P22 material (2.25Cr-1Mo steel) Material Specification

The UNS Number of P22 material is K21590. The EN/ ISO Equivalent material of P22 is 10CrMo9-10 (1.7380).

THE P. Number for welding of P22 material is ‘P5A‘ and Group Number is G1.

It has a primary chemical composition of 2.25% chromium and 1% molybdenum, which gives it excellent resistance to corrosion and oxidation.

The P22 (ASTM A335 P22 Grade, for example) material also has high strength and toughness, making it ideal for use in high-stress applications.

The most common material specifications for P22 ((2.25Cr-1Mo steel) steel are:

  1. ASTM A199, A200, A213: Steel Tubes (T22)
  2. ASTM A336: Forgings (F22, F22a)
  3. ASTM A335: For Pipes (P22 Grade)
  4. ASTM A369: For Forged or Bored Pipe
  5. ASTM A182: fittings and flanges (F22 Grade)
  6. ASTM A234: Welded Pipe Fittings (WP22)

P22 (2.25Cr-1Mo steel) Material Chemical Composition

P22 material (2.25Cr-1Mo steel) is a ferritic steel with a chemical composition of C 0.02, Si 0.35, Mn 1.00, P 0.025, S 0.010, Cr 2.25, Mo 1.00.

It is a low-alloy steel that offers good resistance to oxidation and carburization in the temperature range of 700 to 1000 degrees F (371 to 538 degrees C).

See also  Welding Electrode Types-Welding Rod Number Meaning & Classification

The chemical properties of P22 (2.25Cr-1Mo steel) are listed below:

ElementWeight %
Iron, (Fe)95.1 – 96.75
Carbon (C)0.05 – 0.15
Manganese (Mn)0.30 – 0.60
Silicon (Si)0.50 Maximum
Chromium (Cr)1.90 – 2.60
Molybdenum (Mo)0.87 – 1.13
Sulfur (S)0.025 Maximum
Phosphorus (P)0.025 Maximum
P22 material chemical composition

P22 (2.25Cr-1Mo steel) Material Mechanical Properties

The P22 material (2.25Cr-1Mo steel) is a martensitic stainless steel that has excellent mechanical properties.

It has a tensile strength of 910 MPa, a yield strength of 827 MPa, and a hardness of 241 HB. These properties make it an ideal choice for applications that require high strength and toughness.

PropertyValue
Yield Strength30 Ksi (205 MPa)
Tensile Strength60 Ksi (415 MPa)
Elongation30 % Minimum
Toughness (Charpy V-Notch)Not required
HardnessNot specified
Density 7.8 g/cm3
P22 material Mechanical properties

P22 (2.25Cr-1Mo steel) Material Hardness Range

P22 material is a chromium-molybdenum alloy steel that falls within the ASTM A335 specification. This material has a hardness range that typically falls between Brinell hardness of 210 and 300.

It is often used in high-temperature applications, such as those found in the oil and gas industry.

The alloy’s chromium content helps to increase corrosion resistance, while the molybdenum improves strength and toughness.

For welding of P22 material, maximum hardness permitted are usually 225 BHN or 250 HV as per NACE MR0175.

What is P11 (1.25Cr-0.5Mo steel) and P22 (2.25Cr-1Mo steel) material?

P11 and P22 are both ferritic, Cr-Mo alloy steel grades that are used in high temperature applications.

They are typically used in power plants and other industrial settings where elevated temperatures are present.

See also  How to Weld AISI 4145

These materials have excellent mechanical properties, as well as good resistance to oxidation and corrosion.

P22 (2.25Cr-1Mo steel) Welding Electrode

P22 (2.25Cr-1Mo steel) is a low alloy Cr-Mo steel and can be welded using Stick Welding or SMAW with E80818-B3.

Related reading: Electrode Selection Chart for Welding

P22 (2.25Cr-1Mo steel) Welding Filler Wire

P22 (2.25Cr-1Mo steel) material can be effectively welded using Stick welding (SMAW), TIG Welding, MIG Welding, FCAW and SAW Welding. The mostly used welding electrode or filler wires for P22 material welding are:

  • E8018-B3 (AWS A5.5)
  • ER90S-B3 (AWS A5.28)

Welding Preheat & Interpass Temperature for P22 (2.25Cr-1Mo steel) Welding

Welding preheat shall be applied for welding of P22 material for tacking, cutting, or full welding to ensure the right hardness control and crack free welding joints.

A minimum of 600 °F (315 °C) preheat temperature shall be applied before welding, tacking or cutting of P22 material (2.25Cr-1Mo steel).

This preheat temperature shall be applied a minimum of 3 inches (75 mm) on each side of the welding joint.

The maximum interpass temperature for P22 (2.25Cr-1Mo steel) Material welding is 600 °F (315 °C).

Relating Reading: Welding Preheat: Basics to everything you need to know

Post Weld Heat Treatment (PWHT) for P22 (2.25Cr-1Mo steel) Material

Post Weld Heat Treatment (PWHT) for P22 (2.25Cr-1Mo steel) Material 1275 to 1325(°F) with a minimum 2 hours soaking time.

When maximum creep effect is required, the PWHT temperature range for P22(2.25Cr-1Mo steel) material is 1300 to 1350 (°F) with minimum 2 hours soaking period.

Welding P22 (2.25Cr-1Mo steel) to Carbon Steel

Stick Welding of Welding P22 (2.25Cr-1Mo steel) to Carbon Steel is carried out using E8018-B3 electrode. TIG and MIG welding of P22 alloy is carried out using ER90S-B3 TIG-MIG Filler wire.

See also  Welding ASTM A387 grade 11 (EN 1.7335, DIN 13CrMo4-5)

Welding P22 (2.25Cr-1Mo steel) to Stainless Steel

Stick Welding (SMAW) of P22 material (2.25Cr-1Mo steel) to Stainless Steel shall be carried out using E309L Electrode for service temperature of up to 600 °F (315 °C).

For Service temperature higher than 600 °F (315 °C); P22 or any other Ferritic alloy welding to any other grade of stainless steel shall be carried out using ENiCrFe-3, ENiCrFe-2 or ENiCrFe-2.

TIG Welding of MIG welding of P22 material (2.25Cr-1Mo steel) to Stainless Steel shall be carried out using ER309LSi TIG-MIG Filler wire for service temperature of up to 600 °F (315 °C).

For Service temperatures higher than 600 °F (315 °C); P22 or any other Ferritic alloy welding to any other grade of stainless steel shall be carried out using ERNiCr-3 or ERNiCrMo-3 TIG MIG Filler wire rod.

Welding P22 (2.25Cr-1Mo steel) to P11 (1.25Cr-0.5Mo steel)

Welding P22 (2.25Cr-1Mo steel) to P11 (1.25Cr-0.5Mo steel) shall be carried out using E8018-B3 (Stick Welding-SMAW) or ER90S-B3 Filler wire (TIG & MIG Welding).

Welding P22 (2.25Cr-1Mo steel) to P9 (9Cr-1Mo steel)

Welding P22 (2.25Cr-1Mo steel) to P91 (9Cr-1Mo steel) shall be carried out using E8018-B3 (Stick Welding-SMAW) or ER90S-B3 Filler wire (TIG & MIG Welding).

Does P22 (2.25Cr-1Mo steel) require PWHT?

Yes, P22 material requires mandatory Post-Weld Heat Treatment or PWHT after welding.

Post Weld Heat Treatment (PWHT) for P22 (2.25Cr-1Mo steel) Material 1275 to 1325(°F) with a minimum 2 hours soaking time.

When maximum creep effect is required, the PWHT temperature range for P22(2.25Cr-1Mo steel) material is 1300 to 1350 (°F) with minimum 2 hours soaking period.