Penetrant Removal Methods in PT

After the penetrant has been in contact with the test surface for an acceptable
period, the excess material must be removed from that surface without affecting the
penetrant that has entered a defect.
This is a vital stage for the surface must not be cleaned excessively or defects will
be leached out. However, without proper removal of excess penetrant a high
background will remain, reducing the contrast between potential defects and the test
surface.

The more common methods of penetrant removal with their BS EN 571
classifications are:

  1. Method A Water
  2. Method B Lipophilic emulsifier
  3. Method C Solvent
  4. Method D Hydrophilic remover and water
  5. Method E Water and solvent