Base Metal Repair Procedure by Welding
What is a welding Repair Welding repairs are a common practice as well as it can be uncommon & critical […]
Base Metal Repair Procedure by Welding Read More »
What is a welding Repair Welding repairs are a common practice as well as it can be uncommon & critical […]
Base Metal Repair Procedure by Welding Read More »
What is a Weld map or Weld Trace or Weld Logs? A Weld Map tells what to weld, where to
What are Weld maps or Weld Logs & How to make them? Read More »
What is P Number in Welding? P Number (P mean Parent Metal) in ASME Section IX means the material types
P Number in Welding Read More »
This article explains the various type of Pipes-we hear with their short-form such as ERW Pipe, HFW Pipe, SAW pipe,
ERW Pipe vs. HFW vs. SAW and EFW Pipe Explained Read More »
Pipe thickness Calculation as per ASME B31.3 Determining the minimum necessary pipe wall thickness for a given pipe diameter and
Pipe thickness Calculation as per ASME B31.3 Read More »
What is Hot Tapping? A hot tap, also known as a pressure tap or wet tap, is a method of connecting
Hot Tapping, Purpose, Procedure, Steps Read More »
What is the minimum distance between two welds? Welds should be placed at such a distance that the heat-affected zone
Minimum distance or proximity between two circumferential pipe weld joints Read More »
When purchasing steel products (E.g., Plate, Pipe, Bar), the steel manufacturer must deliver the material certificate, known as Mill Test
Material Test Certificates Explained: 2.1, 2.2, 3.1 and 3.2 Read More »
WELD TESTING Weld testing is a critical and important step in ensuring the quality of welds. There are many different
Weld Testing Methods & Welding Test Types Read More »
Seal Welds Seal welds is a type of weld joint placement that provides an air-tight and water-tight connection for pipes