What is Pickling and Passivation of Stainless Steel?
Discover the importance of pickling and passivation for stainless steel surfaces. Learn how these processes prevent corrosion and enhance durability. …
Discover the importance of pickling and passivation for stainless steel surfaces. Learn how these processes prevent corrosion and enhance durability. …
WRC-1992 Constitute Diagram and its Uses WRC-1992 diagram solves many of the problems faced by the Schaeffler and DeLong diagrams. …
Learn about the Heat Affected Zone (HAZ) in welding and its significance. Understand how welding heat can affect the surrounding …
Delong Diagram: An Introduction Delong Diagram clarifies the Schaeffler diagram (Both are constitute diagrams) using the Nitrogen in the calculation …
What is Lamellar Tearing? Lamellar tearing or Lamellar Cracking is a cracking phenomenon that occurs in thick Al-treated plate that is …
This post covers the effect of heat input in welding on weld metal & HAZ toughness, hardness, microstructure and mechanical …
Understand the importance of dilution in achieving optimal weld quality. Learn how factors such as welding parameters, base metal composition, …
Steel is primarily an alloy of iron and carbon and certain additional elements such as Manganese & silicon. Knowing the …
There are numerous types of Stainless steels and grades that you may deal in day to day life. How you …
Welding of Titanium & Filler wire selection guide Titanium (Ti) is silver-colored metal. It has a strong affinity for oxygen …