Chromoly Steel Aka AISI 4130

What is chromoly steel aka 4130?

Chromoly steel is a low-alloy steel that contains chromium (Cr) and molybdenum (Mo) as main alloying composition. The addition of these two elements gives the steel superior strength and corrosion resistance compared to normal steel.

Let us explore in this post what is Chromoly Steel aka 4130 steel (UNS Number G41300), its properties, comparison with stainless steel and aluminum.

Chromoly steel is often used in the construction of bicycle frames and other high-stress components.

AISI 4130 is the actual designation and grade for the Chromoly Steel. Although term Chromoly is equally used.

While chromoly steel is stronger than traditional steel alloys, it is also more expensive. For this reason, it is not always the best choice for every application. When choosing a steel alloy for a job, it is important to consider the strength requirements and budget restrictions.

Chromoly Steel Composition

Chromoly steel is a medium carbon low alloy steel of chromium and molybdenum, often used in the manufacture of bicycles and other sporting goods.

Chromoly Steel AISI 4130 bicycle frame

The composition of chromoly steel varies depending on the manufacturer, but it typically contains between 0.8% and 1.1% chromium and between 0.15% and 0.25% molybdenum.

Chromoly Steel Composition
Element Weight %
 Carbon %  0.28- 0.33
 Silicon %  0.20- 0.35
 Manganese %  0.40- 0.60
 Chromium %  0.80- 1.10
 Molybdenum %  0.15- 0.25
 Sulfur %  0.040 Max.
 Phosphorus %  0.035 Max.

The mechanical properties of Chromoly Steel (AISI 4130) are covered in the below table.

Chromoly Steel Properties
Property Attributes
Tensile Strength, KSi (MPa) 81 (540) minimum
Hardness 17 HRC
Yield Strength, KSi (MPa) 67 (460)
Density  7.85 g/cm
% Elongation
21.5

Chromoly Steel vs Stainless Steel

Chromoly steel and stainless steel are two of the most common materials used in the manufacturing. Both have their benefits and drawbacks, so it’s important to know which one is right for your needs. Here’s a quick rundown of the differences between chromoly steel and stainless steel:

Chromoly Steel vs Stainless Steel
Chromoly Steel Stainless Steel (Austenitic Stainless Steel)
 It is a Low Alloy Steel  It is a High Alloy Steel
⛔ Low Corrosion resistance  High Corrosion resistance
 ✅ Cheaper ⛔ Costly
✅ Density 7.85 g/cm ⛔ Density 8.00 g/cm
✅High Yield Strength
 Low Yield Strength
✅ High Tensile Strength  Low tensile Strength
✅ Change in properties by heat treatment  No response to heat treatment
✅ High strength to weight ratio  Low strength to weight ratio
 Less aesthetic  ✅ Highly aesthetic, surface finish
 Moderate weldability ✅ Very good weldability

Chromoly Steel vs Aluminum

There are many factors to consider when choosing between chromoly steel and aluminum based on their physical, mechanical and chemical properties. Here are a few key considerations for Chromoly Steel vs Aluminum:

-Weight: Chromoly steel is significantly heavier than aluminum, making it more difficult to work with.

-Cost: Chromoly steel is typically cheaper than Aluminum.

-Strength: Chromoly steel is stronger and tougher than aluminum, making it better suited for projects that require high levels of strength and durability.

Chromoly Steel vs Aluminum
Chromoly Steel Aluminum
 It is a Low Alloy Steel Aluminum available as pure metal and alloys of Aluminum
⛔ Low Corrosion resistance  High Corrosion resistance
 ✅ Cheaper ⛔ Costly
⛔ Density 7.85 g/cm  Density 2.7 g/cm (Lightweight)
✅High Yield & Tensile Strength
 Low Yield & Tensile Strength
✅ High toughness & hardness  Low toughness & soft
✅ Change in properties by heat treatment  No response to heat treatment
✅ High strength to weight ratio  Low strength to weight ratio
✅ Reduce size for construction due to high strength ⛔Need larger sizes for construction due to low strength
 Moderate weldability ✅ Good weldability

Aluminum is a soft metal that is often used in the construction of aircraft. It is lightweight and has a high strength-to-weight ratio. However, aluminum is not as strong as steel and is not as resistant to wear and tear.

When choosing between chromoly steel and aluminum, weight, cost, and strength are all important factors to consider. In general, aluminum is lighter and costly than chromoly steel, but chromoly steel is stronger.

AISI 4130 Aka Chromoly steel

AISI 4130 is a chromium-molybdenum alloy steel. It has high strength and toughness, weldability and machinability. The UNS Number for AISI 4130 steel is G41300.

Read my article on AISI 4130 Chromoly steel welding Guide.

4130 alloy steel is used for structural applications such as aircraft frames and racecar frames. It is also used for making gears, shafts and other power transmission parts.

This steel can be heat treated for higher strength levels due to its high carbon content that gives is more allotropic transformation.

 The alloy has good ductility in the annealed condition but can become brittle when quench hardened. Due to this the steel is supplied in Quench and tempered condition.

AISI 4130 steel is made using melting practices that include electric arc furnace, vacuum degassing, and ladle metallurgy. The steel is then cooled to various temperatures to achieve different properties. For example, it can be cooled rapidly to improve its hardness or slowly to improve its ductility.

Is Chromoly stronger than regular steel?

Chromoly steel is a type of low-alloy steel that gets its name from a combination of the words “chromium” and “molybdenum.” Chromoly steel is often used in high-performance applications because it has a higher strength-to-weight ratio than regular steel, making it more durable.

So, is chromoly stronger than regular steel? The answer is yes, chromoly is stronger than regular steel. But it’s also worth noting that chromoly steel is not as strong as some other types of steels, such as tool steels.

The addition of chromium and molybdenum elements makes chromoly stronger and more resistant to wear than regular steel.
While chromoly is stronger than regular steel, it is also more expensive. This makes it a good choice for applications where strength is important, but cost is not a major concern.

Still, chromoly has many benefits that make it ideal for certain applications. For example, because it’s lighter than regular steel, chromoly can help reduce fuel consumption in vehicles.

Read more:


Related Posts:

See also  Heat Affected Zone or HAZ in Welding Explained

Material Welding is run by highly experienced welding engineers, welding trainers & ASNT NDT Level III bloggers. We strive to provide most accurate and practical knowledge in welding, metallurgy, NDT and Engineering domains.