Best Welding Rod for Cast Steel

Best Welding Rod for Cast Steel

The best welding rod for cast steel depends on two main factors: the application of the weld and the type of base material.

There are many different types of welding rods available, including mild steel electrodes, stainless steel electrodes and nickel-based alloy electrodes.

Each welding rod has its specific features that must be considered in order to select the best rod for any given application.

Best Welding Rod for Cast Steel welding

Best stick welding Rods for Cast Steel Welding

6013 Welding Rod

6013 welding rod is a type of mild steel electrode that is commonly used for welding in the flat and horizontal positions.

Forney E6013
Welding Rod,
3/32-Inch
hobart-e7018Hobart E6013
Welding Rod

It is known for its smooth arc action, easy slag removal, and high deposition rate. It is often used for welding sheet metal, structural steel, and other low-carbon steels. It is also suitable for welding in both AC and DC current.

7018 Welding Rod

For welding cast steel, 7018 welding rod may be a better choice than 6013 welding rod in term of high strength and low hydrogen content.

Note that Cast steel is similar to carbon steel with low carbon content, but it’s in a casting form.

hobart-e7018Hobart 7018 Stick, 1/8-10lbs
lincoln welding rodLincoln E7018 Stick Electrode,
1/8 in. dia
E6010Forney E7018 Welding Rod,
5/32-Inch

7018 welding rod provides a deep penetration that can help to fill any porosity or voids in the cast steel, which is common in casting process.

7015 Welding Rod

7015 welding rod is a low hydrogen electrode that is similar to 7018, but it is designed to have a faster freezing slag, which allows for higher welding speeds and more penetration in welding.

See also  E7024 Welding Electrode: Everything You need to know

Read more: E7015 Welding Rod Properties & Uses.

It is also designed to have a lower hydrogen content, which makes it less susceptible to cracking and porosity.

For welding cast steel, 7015 welding rod is  a good choice as it is designed to work with low hydrogen and high carbon steels.

It’s also known to have good impact toughness and it can provide good penetration and good bead appearance.

Best TIG welding Rods for Cast Steel Welding

The best TIG welding rods for cast steel welding would depend on the specific type of cast steel and the desired properties of the welded joint.

For carbon steel base cast steel you can use following welding rods:

ER70S-2 for Cast Steel Welding

ER70S-2 can be used for welding cast steel and some types of cast steel that has low carbon content and low alloy.

Read more: ER70S-2 TIG wire Properties.

The wire has triple deoxidizer that prevent porosity as well as give good weldability on rusty cast steel surface.

ER70S-2ER70S-2 TIG wire.

It can be used for DCEP polarity in TIG with pure argon gas shielding. The strength of ER70S-2 is higher and also having very good weldability.

ER70S-6 for Cast Steel Welding

ER70S-6 TIG rod for cast steel welding is an excellent choice for welders who are looking for a rod to make clean and reliable welds.

This type of rod is highly popular among professionals due to its good weldability and high tensile strength.

ImageProductDetails  
buy ER70S-6 tig mig wireYESWELDER MAKE ER70S-6, Diameter .035-InchHigh Quality, Best Price, Free Delivery
ER70S-2Kiswel Make ER70S-2 TIG WireMake: Kiswel
Made in Korea
High-Quality TIG wires

It can be used in both manual and automated welding processes, making it very versatile and suitable for a welding cast steel.

See also  Top 20 very useful questions answers for Welders

The main advantages of using ER70S-6 TIG rod for cast steel welding include: good mechanical properties, low spatter characteristics, good impact resistance, great wetting action and improved bead appearance.

The low carbon content also results in better corrosion resistance compared to other wires.

Additionally, the deposits created by this type of rod are quite smooth which helps in reducing post-weld cleaning time.

Best MIG welding Rods for Cast Steel Welding

When it comes to MIG welding rods, there are many options available for cast steel welding. Two of the best rods are ER70S-6 and ER70S-2 wires.

These two wires offer excellent weld deposits that will enable you to make strong and reliable welds on cast steel materials.

The ER70S-6 wire is a copper coated mild steel wire with high levels of manganese and silicon that produces an incredibly strong weld deposit.

It also has higher amounts of deoxidizers, which help to reduce porosity in welds that may be exposed to moisture or corrosion over time.

The ER70S-2 wire is ideal for welding Cast Steel components since it has a higher amount of manganese and silicon with added titanium than the other rods, which gives it superior strength & ability to weld on rusty surfaces.

Best Gasless MIG welding wire for Cast Steel Welding

When selecting a gasless MIG welding wire, opt for one made from solid core flux-cored steel and designed specifically for cast steel applications.

Look for wires that are compatible with both AC and DC power sources and offer an excellent combination of strength and ductility, as well as smooth feeding characteristics and good slag removal.

See also  What is MIG Welding
NR-211-MP-1NR-211-MP-1
(AWS E71T-11)
Made in USA
E71T-GS welding wireForney Flux Core
Mig Wire,
E71TGS,
030-Diameter

E71T-8 and E71T-11 are gasless, self-shielded flux-cored wires that are commonly used for MIG welding low-alloy and carbon steels.

Both wires do not require an external shielding gas and can be used in a variety of positions.

E71T-8 typically provides a smooth, stable arc and a good bead appearance, while E71T-11 has a higher level of deoxidizers and provides a better penetration and less spatter than E71T-8.

The E71T-8, and E71T-11 gasless MIG wires are great options for performing cast steel welding because they can provide superior strength, excellent corrosion resistance, and good ductility in the welded areas.


Material Welding is run by highly experienced welding engineers, welding trainers & ASNT NDT Level III bloggers. We strive to provide most accurate and practical knowledge in welding, metallurgy, NDT and Engineering domains.