Salt spray testing

ASTM B117 Salt Spray Test

Salt Spray Test Salt spray testing (or salt spray test) is a standardized test and an important tool used to evaluate the corrosion …

Read more

Fatigue-damage

What is Fatigue Failure?

Fatigue Failure in Metals Fatigue failure is a failure mechanism occurring among metals, non-metals and alloys, leading to the weakening …

Read more

HY80 Steel Welding

Welding HY80 Steel

Welding HY80 Steel HY80 steel is a high strength and high strength to weight ration low alloy steel that has …