Welding 1018 Steel

Welding 1018 Steel

Welding 1018 steel can be a daunting task, but with the right knowledge and equipment, it can be done with relative ease.

This article will cover the basics of welding 1018 steel, providing resources for those less familiar with this type of metal. We will discuss the chemical composition of the metal, as well as the best practices for welding it.

1018 Steel Weldability

Weldability is an important factor to consider when it comes to selecting suitable materials for fabrication.

1018 steel, a popular grade of low carbon steel, offers excellent weldability and machinability. It is often used in the construction of structures and components, as well as in repair and maintenance work.

When it comes to welding 1018 steel, the most important thing to remember is that it must be well preheated before any welding takes place, especially when welding thick parts. This will help prevent any cracking.

Welding-1018-Steel

1018 Steel Chemical and Mechanical Properties

1018 steel chemical and mechanical properties are listed below:

Chemical Properties:

  • Carbon: 0.15-0.20%
  • Manganese: 0.60-0.90%
  • Phosphorus: 0.04% max
  • Sulfur: 0.05% max
aisi-1018 steel

Mechanical Properties (annealed) typical values:

  • Tensile Strength: 58,000 – 79,800 psi
  • Yield Strength: 42,000 – 64,800 psi
  • Elongation: 15% min
  • Reduction of Area: 40% min
  • Hardness (Brinell): 120 – 180

Stick Welding 1018 Steel

When stick welding 1018 steel, it’s important to use the correct electrode. A carbon steel electrode, such as an E7016 or E7018, is a good choice for welding 1018 steel.

You can also use E6011 or E6013 electrodes but their strength is lower than the E7018 welding rod.

It’s also important to use the correct welding technique. Such as stringer bead, that help to control the weld distortion.

E7018 or E7016 can be used with DCEP Polarity. Check this post on welding polarity type for different welding rods.

See also  Overhead Welding tips and technique for Stick and MIG welding

Make sure to clean the steel of any oil, paint, rust, or other contaminants before welding. This will ensure a strong, clean weld and good quality.

mig welding 1018 steel

MIG welding, also known as Gas Metal Arc Welding (GMAW), is another method that can be used to weld 1018 steel. MIG welding is a semi-automatic or automatic process that uses a continuous wire feed and an inert gas to shield the weld.

When MIG welding 1018 steel, it’s important to use the correct welding wire and gas. A mild steel MIG wire, such as an ER70S-2 or ER70S-6, is a good choice for welding 1018 steel.

ER70S-2 is a wire that is designed for welding low and medium carbon steels and is recommended for welding 1018 steel. It has a high level of deoxidizing agents than the ER70S-6, which makes it suitable for welding even on rusty surfaces.

ER70S-6 is another popular MIG welding wire for carbon steels.

The gas commonly used for MIG welding is a mixture of argon and CO2 (75% Argon and 25% CO2) or 100% Argon. This gas is used to shield the weld and prevent oxidation and other forms of contamination.

When MIG welding 1018 steel, it’s important to use the correct welding technique and maintain a consistent travel speed.

A spray transfer technique is often used when MIG welding 1018 steel, although you should use short-circuit transfer for sheet metal jobs.

It’s also important to use the correct amperage to match the thickness of the material and the wire being used. A good rule of thumb is to use an amperage that is 1 amp per 0.001 inches of material thickness.

Tig welding 1018 steel

For TIG welding 1018 steel, you can use the same filler wire as MIG welding. Either ER70S-2 or ER70S-6 type.

See also  Welding Electrode Types-Welding Rod Number Meaning & Classification

Sometimes when welding 1018 steel with TIG, a welder may face a lot of porosity.

This could be uncleaned surface or insufficient gas coverage. In such situations, use ER70S-2 wire and make sure surface is clean with sufficient gas shielding.

The gas commonly used for TIG welding is a mixture of argon and helium. A pure tungsten electrode, such as a 2% thoriated or ceriated, is a good choice for welding 1018 steel.

What is the proper smaw electrode to use for welding 1018 to a36 steel?

When welding 1018 steel to A36 steel using the stick welding or SMAW (Shielded Metal Arc Welding) process, the proper electrode to use would be an E7018 electrode.

The E70XX series of electrodes (e.g., E7016 or E7018) are low-hydrogen, mild steel electrodes that are commonly used for welding low-carbon steels such as 1018 and A36.

For welding in all positions, an E7018 electrode is a good choice. It’s a low-hydrogen electrode that produces a deep penetrating, high-strength weld with good impact resistance.

welding 1018 to 4140

Welding 1018 steel to 4140 steel can be done using the  stick welding or SMAW (Shielded Metal Arc Welding) process, but it is important to keep in mind that 4140 steel is a alloy steel that is harder and stronger than 1018 steel.

This means that the welding process will be more challenging, and special care must be taken to ensure a successful weld.

The proper electrode to use for welding 1018 to 4140 would be an E70XX electrode, specifically an E7018.

TIG or MIG welding of 1018 steel to 4140 steel is carried out using ER70S-2 or ER70S-6 filler wire rod. For TIG welding use pure argon gas shielding while for MIG welding of 1018 to 4140, go for 75-25 welding gas.

It’s essential to preheat the material especially 4140 steel before welding. Post heat treatment can be given to reduce the residual stresses and weld hardness.

See also  Types of Cast Irons, Identification & their Welding

Welding 1018 cold rolled steel

1018 cold rolled steel is a low carbon steel with good weldability properties. It can be welded using any common welding method, including stick welding, MIG welding, and TIG welding.  

However, it is important to use the proper welding technique and filler metal as explained in this article.

welding 1018 and 304 stainless steel

When welding carbon steel to stainless steel, it is important to use a filler metal that is compatible with both materials. One option is to use a 309L filler metal, which is designed for welding dissimilar steels.

Additionally, proper cleaning of the surfaces to be welded is crucial to ensure a sound weld. The stainless steel must be cleaned to remove any surface contaminants such as oil, grease or other impurities.

For stick welding 1018 to 304 stainless steel, you can use E309L-16 welding rod.

For TIG welding 1018 to 304 stainless steel, go for ER309L and ER309LSi for MIG welding.

 TIG welding need pure argon gas shielding while for MIG welding, use 98%Ar+2%O2 welding gas.

Welding 1018 to 572 gr 59

Welding 1018 cold rolled steel to 572 Gr. 59 steel using E7018 or E8018-G rod can be done. 7018 and E8018-G are both low-hydrogen, iron powder electrode which is designed for welding carbon and low alloy steels and can be used with both DC and AC power sources.

Read more: How to weld astm a572


Material Welding is run by highly experienced welding engineers, welding trainers & ASNT NDT Level III bloggers. We strive to provide most accurate and practical knowledge in welding, metallurgy, NDT and Engineering domains.