Skip to content

Material Welding

  • WELDING KNOWLEDGE
    • Welding Inspection
    • Welding Processes
    • Welding Engineering
      • Welding Metallurgy
      • Welding Design
    • AWS-CWI examination
    • BPVC ASME Code knowledge
    • Metallurgy
      • Ferrous and Non-Ferrous materials
      • Heat Treatment of Metals
      • Destructive Testing
      • Failure Analysis
      • Corrosion Technology
      • Buy Online Welding Tools & Gauges
  • Courses
  • Free Calculators
  • Non-destructive Testing
    • Liquid Penetrant Testing
    • Magnetic Particle Testing (MT)
    • Radiography Testing (RT)
    • Ultrasonic Testing (UT)
    • Visual Testing (VT)
    • Advance NDT Method
  • How to Weld
    • How to Weld Aluminum
    • How to Weld Stainless Steel
    • Welding of Cr-Mo Steels
    • Welding of Low Alloy Steels
    • Welding of Non-ferrous metals
  • WELDING VIDEOS
    • AWS-CWI TRAINING EXAM VIDEOS
    • WELDING DEFECTS VIDEOS
    • NDT VIDEOS-ASNT EXAMS
    • WELDING PROCESSES
    • WELDING SYMBOLS & JOINTS

Welding Metallurgy

Online Welding-NDT Calculators

Free Welding- NDT Online Calculators

preheat in welding

Preheating in Welding: Basics to everything you need to know

What is Preheating in Welding? Preheating in Welding involves heating the base metal surrounding the weld joint, to a specific …

Read more

welding of cast iron

Types of Cast Irons, Identification & their Welding

Detailed Guide on Cast Iron types, their Identification & Welding Cast irons are assumed to have good weldability but it …

Read more

temper bead welding

Temper Bead Welding (TBW)/ Controlled Weld Deposition (CWD)

What is temper Bead Welding (TBW) or Controlled Weld Deposition (CWD) Performing welding repair on materials that are exposed to …

Read more

Schaeffler Diagram and its practical uses

What is Schaeffler Diagram? The Schaeffler diagram is an important tool for predicting the constitution of your stainless steel weld …

Read more

crack in aluminum

How to avoid weld cracking in 2000 Series-2011 & 2014 Aluminum alloys welding

Aluminum 2000 properties 2000 Series aluminum is a copper base Aluminum alloy having high strength and hardness with good machinability. …

Read more

hydrogen_crack_haz

What is Hydrogen Cracking or Delayed Cracking or Cold Cracking?

What is Hydrogen cracking or cold cracking or Delayed Cracking? Hydrogen Induced Cracking (HIC) which is commonly known as Hydrogen …

Read more

Ferrite Testing calculate ferrite content in stainless steel duplex stainless steel

How to Calculate Ferrite Content in Stainless Steel?

Importance of Ferrite in Austenitic & Duplex stainless steel welds A characteristic of austenitic stainless is their susceptibility to hot-short …

Read more

Heat input in welding

Heat Input in Welding, Formulas, Free Online Calculator, and Units

Heat Input in Welding is an important factor for the resultant weld deposit properties. So, it is crucial to use …

Read more

Welding Electrode Types-Welding Rod Number Meaning & Classification

Explore the world of welding electrode types and understand the meaning and classification of welding rod numbers. Gain valuable insights …

Read more

Older posts
Newer posts
← Previous Page1 … Page13 Page14 Page15 Page16 Next →
  • API 570 Closed Book Questions
  • NACE CIP Level 2 Exam Questions with Answers and Explanations
  • CSWIP 3.1 Exam Questions with Answers and Explanations
  • Top Questions for the Certified Manufacturing Engineer (CMfgE) Exam
  • Free Practice Questions for the Certified Manufacturing Engineer (CMfgE) Examination

MaterialWelding.com is a participant in the Amazon Services LLC Associates Program, an affiliate advertising program designed to provide a means for sites to earn advertising fees by advertising and linking to Amazon.com.

  • YouTube
  • LinkedIn
  • Facebook
  • Pinterest

Footer

  • Material Welding: about us
  • Privacy Policy
  • Contact Us
Copyright © 2023 !www.materialwelding.com!